General
Property | Value | Comment |
---|---|---|
Densidad | 2.6 - 2.7 g/cm³ Show Material materials with Densidad of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | ||
Dureza Brinell | 90.0 [-] Show Material materials with Dureza Brinell of 90.0 [-] | T4 | GB 1173 | |
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | ||
Resistencia a la tracción | 290.0 MPa Show Material materials with Resistencia a la tracción of 290.0 MPa | T4 | GB 1173 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Conductividad térmica | 60.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Temperatura de fusión | 450.0 - 640.0 °C Show Material materials with Temperatura de fusión of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Berilio | 0.03 - 0.1 % Show Material materials with Berilio of 0.03 - 0.1 % | T4 | GB 1173 |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | T4 | GB 1173 |
Magnesio | 7.5 - 9.0 % Show Material materials with Magnesio of 7.5 - 9.0 % | T4 | GB 1173 |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T4 | GB 1173 |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | T4 | GB 1173 |
Titanio | 0.1 - 0.2 % Show Material materials with Titanio of 0.1 - 0.2 % | T4 | GB 1173 |
Zinc | 1.0 - 1.5 % Show Material materials with Zinc of 1.0 - 1.5 % | T4 | GB 1173 |