General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 - 8.4 g/cm³ Show Material materials with Densidad of 7.75 - 8.4 g/cm³ | Typical for Nickel Chromium Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 150 GPa Show Material materials with Módulo elástico of 150 GPa | Typical for Nickel Chromium Iron Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Iron Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Iron Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Iron Alloy |
Temperatura de fusión | 1200 - 1480 °C Show Material materials with Temperatura de fusión of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.05 - 0.12 % Show Material materials with Carbono of 0.05 - 0.12 % |
Cerio | 0.03 - 0.09 % Show Material materials with Cerio of 0.03 - 0.09 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 26 - 29 % Show Material materials with Cromo of 26 - 29 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 21 - 25 % Show Material materials with Hierro of 21 - 25 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 45 % Show Material materials with Níquel of 45 % |
Otro | In the product standard DIN EN 10095 slightly different limits are defined., A maximum value of 1.5 % Co, counted as Ni, is permitted. The identification of Co is not required. |
Silicona | 2.5 - 3 % Show Material materials with Silicona of 2.5 - 3 % |