Nickel Chromium Iron Alloy
Sanicro® 28Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable ferrítico
Sandvik 4C54Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2707 HD™Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2906™Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1NiCrMoCu31-27-4 solution annealed (+AT)Acero inoxidable dúplex
S32550 / AMAZON 256 Duplex Stainless SteelAcero inoxidable dúplex
S32760 / SEACOL-760 Duplex Stainless SteelAcero inoxidable austenítico
EN 10272 Grade X1NiCrMoCu31-27-4 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)