Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 % Show Material materials with Aluminio of 0.3 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.05 - 0.12 % Show Material materials with Carbono of 0.05 - 0.12 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 26 - 29 % Show Material materials with Cromo of 26 - 29 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 21 - 25 % Show Material materials with Hierro of 21 - 25 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 40 % Show Material materials with Níquel of 40 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 2.5 - 3 % Show Material materials with Silicona of 2.5 - 3 % |