Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cromo | 29 - 31 % Show Material materials with Cromo of 29 - 31 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 10 - 12 % Show Material materials with Molibdeno of 10 - 12 % |
Níquel | 53 % Show Material materials with Níquel of 53 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Vanadio | 0.4 % Show Material materials with Vanadio of 0.4 % |