Acero inoxidable endurecido por precipitación
UGI® HT286 Annealed and Cold Drawn and AgedSuministrada por:
UgitechAcero inoxidable austenítico
EN 10216-5 Grade X10CrNiMoMnNbVB15-10-1 solution annealed (+AT)Acero inoxidable martensítico
EN 10269 Grade X12CrNiMoV12-3 quenched and tempered (+QT)Acero inoxidable martensítico
EN 10090 Grade X85CrMoV18-2 quenched and tempered (+QT)Acero inoxidable endurecido por precipitación
UGI® HT286 Annealed and Cold DrawnSuministrada por:
UgitechAcero inoxidable austenítico
ASTM A453 Grade 651 Class AAcero inoxidable austenítico
EN 10269 Grade X10CrNiMoMnNbVB15-10-1 solution heat-treated and warm worked (+AT+WW)Acero inoxidable martensítico
ASTM A565 Grade XM-32 Heat treated for high-temperature serviceAcero inoxidable martensítico
DIN 17480 Grade X85CrMoV18-2 quenched and tempered (+QT)Acero para herramientas y maquinaria
ISO 4957 Grade X32CrMoV3-3 soft annealed (+A)Acero inoxidable martensítico
EN 10269 Grade X12CrNiMoV12-3 quenched and tempered (+QT1)Acero para herramientas y maquinaria
ISO 4957 Grade X38CrMoV5-1 soft annealed (+A)Acero para herramientas y maquinaria
ISO 4957 Grade X165CrMoV12 soft annealed (+A)Acero para herramientas y maquinaria
Thermodur 2343 EFS PlateSuministrada por:
Deutsche Edelstahlwerke (DEW)Acero para herramientas y maquinaria
Thermodur 2343 EFS Superclean PlateSuministrada por:
Deutsche Edelstahlwerke (DEW)Acero inoxidable martensítico
ASTM A565 Grade XM-32 AnnealedAcero inoxidable endurecido por precipitación
EN 10269 Grade X6NiCrTiMoVB25-15-2 solution heat-treated and precipitation hardened (+AT+P)8000 Series
AA Standards Grade 8022