Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.02 - 0.1 % Show Material materials with Carbono of 0.02 - 0.1 % |
Cobalto | 27 - 32 % Show Material materials with Cobalto of 27 - 32 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 26 - 29 % Show Material materials with Cromo of 26 - 29 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3.5 % Show Material materials with Hierro of 3.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.7 % Show Material materials with Molibdeno of 0.7 % |
Niobio | 0.3 % Show Material materials with Niobio of 0.3 % |
Níquel | 30 % Show Material materials with Níquel of 30 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 2.4 - 3 % Show Material materials with Silicona of 2.4 - 3 % |
Titanio | 0.2 - 0.6 % Show Material materials with Titanio of 0.2 - 0.6 % |
Wolframio | 0.5 % Show Material materials with Wolframio of 0.5 % |