Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobalto | 2.5 % Show Material materials with Cobalto of 2.5 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 14.5 - 16.5 % Show Material materials with Cromo of 14.5 - 16.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 4 - 7 % Show Material materials with Hierro of 4 - 7 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 15 - 18 % Show Material materials with Molibdeno of 15 - 18 % |
Níquel | 50 % Show Material materials with Níquel of 50 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Vanadio | 0.4 % Show Material materials with Vanadio of 0.4 % |
Wolframio | 3 - 4.5 % Show Material materials with Wolframio of 3 - 4.5 % |