General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H16 | EN 573-3, EN 485 | ||
20.0 °C | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Dureza Brinell | 52.0 [-] Show Material materials with Dureza Brinell of 52.0 [-] | H16 | EN 573-3, EN 485 | |||
20.0 °C | 40.0 [-] Show Material materials with Dureza Brinell of 40.0 [-] | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | ||
20.0 °C | 52.0 [-] Show Material materials with Dureza Brinell of 52.0 [-] | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
Elongación | 1.0 % Show Material materials with Elongación of 1.0 % | H16 | EN 573-3, EN 485 | A50 | ||
2.0 % Show Material materials with Elongación of 2.0 % | H16 | EN 573-3, EN 485 | A50 | |||
3.0 % Show Material materials with Elongación of 3.0 % | H16 | EN 573-3, EN 485 | A50 | |||
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip | A10 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | A10 | |
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | ||
Módulo de cizallamiento | 26.1 GPa Show Material materials with Módulo de cizallamiento of 26.1 GPa | H16 | EN 573-3, EN 485 | |||
20.0 °C | 25.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 GPa | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube | ||
Módulo elástico | 69.5 GPa Show Material materials with Módulo elástico of 69.5 GPa | H16 | EN 573-3, EN 485 | |||
20.0 °C | 60.0 - 65.0 GPa Show Material materials with Módulo elástico of 60.0 - 65.0 GPa | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 140.0 MPa Show Material materials with Resistencia a la tracción of 140.0 MPa | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | |
20.0 °C | 165.0 - 205.0 MPa Show Material materials with Resistencia a la tracción of 165.0 - 205.0 MPa | H16 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Sheet, Flat, Strip | ||
Ángulo de flexión a 90° | 1.0 °/t Show Material materials with Ángulo de flexión a 90° of 1.0 °/t | H16 | EN 573-3, EN 485 | |||
1.5 °/t Show Material materials with Ángulo de flexión a 90° of 1.5 °/t | H16 | EN 573-3, EN 485 | ||||
2.0 °/t Show Material materials with Ángulo de flexión a 90° of 2.0 °/t | H16 | EN 573-3, EN 485 | ||||
2.5 °/t Show Material materials with Ángulo de flexión a 90° of 2.5 °/t | H16 | EN 573-3, EN 485 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 879.0 J/(kg·K) Show Material materials with Calor específico of 879.0 J/(kg·K) | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube | |
Coeficiente de dilatación térmica | -50 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | |
-50.0 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
20 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
20 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
20 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
20 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
100 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
100.0 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
200 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
200.0 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
300 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
300.0 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | H16 | EN 573-3, EN 485, DIN 1725-1, EN 573-4 | Sheet, Flat, Strip, Tube | ||
Conductividad térmica | 20.0 °C | 160.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 160.0 - 220.0 W/(m·K) | H16 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Sheet, Flat, Strip, Tube | |
Temperatura de fusión | 630.0 - 650.0 °C Show Material materials with Temperatura de fusión of 630.0 - 650.0 °C | H16 | EN 573-3, EN 485 | |||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 23000000.0 - 31000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 31000000.0 S/m | H16 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Sheet, Flat, Strip, Tube |
Resistividad eléctrica | 3.23e-08 - 4.35e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.23e-08 - 4.35e-08 Ω·m | H16 | EN 573-3, EN 485 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
0.2 % Show Material materials with Cobre of 0.2 % | H16 | EN 573-3, EN 485 | ||
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | H16 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Sheet, Flat, Strip, Tube |
Hierro | 0.45 % Show Material materials with Hierro of 0.45 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
0.70 % Show Material materials with Hierro of 0.70 % | H16 | EN 573-3, EN 485 | ||
Magnesio | 0.7 - 1.1 % Show Material materials with Magnesio of 0.7 - 1.1 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
1.1 - 1.8 % Show Material materials with Magnesio of 1.1 - 1.8 % | H16 | EN 573-3, EN 485 | ||
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
0.3 % Show Material materials with Manganeso of 0.3 % | H16 | EN 573-3, EN 485 | ||
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
0.4 % Show Material materials with Silicona of 0.4 % | H16 | EN 573-3, EN 485 | ||
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H16 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip, Tube |
0.25 % Show Material materials with Zinc of 0.25 % | H16 | EN 573-3, EN 485 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |