General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H18 | EN 573-3, EN 1301 | ||
20.0 °C | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 60.0 [-] Show Material materials with Dureza Brinell of 60.0 [-] | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | |
Elongación | 3.0 % Show Material materials with Elongación of 3.0 % | H18 | EN 573-3, EN 1301 | |||
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | A10 | |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | ||
Módulo de cizallamiento | 20.0 °C | 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.5 GPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H18 | EN 573-3, EN 1301 | |||
20.0 °C | 65.0 - 70.0 GPa Show Material materials with Módulo elástico of 65.0 - 70.0 GPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 245.0 MPa Show Material materials with Resistencia a la tracción of 245.0 MPa | H18 | EN 573-3, EN 1301 | |||
20.0 °C | 220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | |
Coeficiente de dilatación térmica | 20 °C | 2.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.38e-05 1/K | H18 | EN 573-3, EN 1301 | ||
100 °C | 2.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.38e-05 1/K | H18 | EN 573-3, EN 1301 | |||
Conductividad térmica | 20.0 °C | 135.0 - 167.0 W/(m·K) Show Material materials with Conductividad térmica of 135.0 - 167.0 W/(m·K) | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | |
Temperatura de fusión | 560.0 - 655.0 °C Show Material materials with Temperatura de fusión of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 22000000.0 - 26000000.0 S/m Show Material materials with Conductividad eléctrica of 22000000.0 - 26000000.0 S/m | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | |
Resistividad eléctrica | 3.3e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Hierro | 0.45 % Show Material materials with Hierro of 0.45 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Tube |
0.45 % Show Material materials with Hierro of 0.45 % | H18 | EN 573-3, EN 1301 | ||
Magnesio | 1.4 - 2.1 % Show Material materials with Magnesio of 1.4 - 2.1 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Manganeso | 0.25 % Show Material materials with Manganeso of 0.25 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H18 | DIN 1725-1, EN 573-3, EN 573-4, EN 1301 | Tube |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |