General
Property | Value | Condition | Related Standards |
---|---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | T3510 | EN 573-3, EN 754 |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||
Módulo de cizallamiento | 27.2 GPa Show Material materials with Módulo de cizallamiento of 27.2 GPa | T3510 | EN 573-3, EN 754 | |
Módulo elástico | 72.5 GPa Show Material materials with Módulo elástico of 72.5 GPa | T3510 | EN 573-3, EN 754 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||
Resistencia a la tracción | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T3510 | EN 573-3, EN 754 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium | |||
Coeficiente de dilatación térmica | 20 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T3510 | EN 573-3, EN 754 | |
100 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T3510 | EN 573-3, EN 754 | ||
Conductividad térmica | 130.0 - 200.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 200.0 W/(m·K) | T3510 | EN 573-3, EN 754 | ||
Temperatura de fusión | 512.0 - 650.0 °C Show Material materials with Temperatura de fusión of 512.0 - 650.0 °C | T3510 | EN 573-3, EN 754 |
Eléctrico
Property | Value | Condition | Related Standards |
---|---|---|---|
Conductividad eléctrica | 18000000.0 - 28000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 28000000.0 S/m | T3510 | EN 573-3, EN 754 |
Resistividad eléctrica | 3.57e-08 - 5.56e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.57e-08 - 5.56e-08 Ω·m | T3510 | EN 573-3, EN 754 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 3.5 - 4.5 % Show Material materials with Cobre of 3.5 - 4.5 % | T3510 | EN 573-3, EN 754 |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T3510 | EN 573-3, EN 754 |
Hierro | 0.70 % Show Material materials with Hierro of 0.70 % | T3510 | EN 573-3, EN 754 |
Magnesio | 0.4 - 1.0 % Show Material materials with Magnesio of 0.4 - 1.0 % | T3510 | EN 573-3, EN 754 |
Manganeso | 0.4 - 1.0 % Show Material materials with Manganeso of 0.4 - 1.0 % | T3510 | EN 573-3, EN 754 |
Silicona | 0.2 - 0.8 % Show Material materials with Silicona of 0.2 - 0.8 % | T3510 | EN 573-3, EN 754 |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T3510 | EN 573-3, EN 754 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: good | |
Brazing | hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: acceptable, soft brazing with flux: not suitable | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) acceptable (O) / acceptable (O) |