General
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Dureza Brinell | 26.0 [-] Show Material materials with Dureza Brinell of 26.0 [-] | H22 | EN 573-3, EN 485 | |||
20.0 °C | 28.0 [-] Show Material materials with Dureza Brinell of 28.0 [-] | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | ||
Elongación | 8.0 % Show Material materials with Elongación of 8.0 % | H22 | EN 573-3, EN 485 | A50 | ||
9.0 % Show Material materials with Elongación of 9.0 % | H22 | EN 573-3, EN 485 | A50 | |||
11.0 % Show Material materials with Elongación of 11.0 % | H22 | EN 573-3, EN 485 | A50 | |||
13.0 % Show Material materials with Elongación of 13.0 % | H22 | EN 573-3, EN 485 | A50 | |||
15.0 % Show Material materials with Elongación of 15.0 % | H22 | EN 573-3, EN 485 | A50 | |||
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | A10 | |
20.0 °C | 15.0 % Show Material materials with Elongación of 15.0 % | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | ||
Módulo de cizallamiento | 20.0 °C | 25.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 GPa | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H22 | EN 573-3, EN 485 | |||
20.0 °C | 60.0 - 70.0 GPa Show Material materials with Módulo elástico of 60.0 - 70.0 GPa | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 80.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 120.0 MPa | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip | |
Ángulo de flexión a 180° | 0.5 °/t Show Material materials with Ángulo de flexión a 180° of 0.5 °/t | H22 | EN 573-3, EN 485 | |||
Ángulo de flexión a 90° | 0.5 °/t Show Material materials with Ángulo de flexión a 90° of 0.5 °/t | H22 | EN 573-3, EN 485 | |||
1.0 °/t Show Material materials with Ángulo de flexión a 90° of 1.0 °/t | H22 | EN 573-3, EN 485 | ||||
2.0 °/t Show Material materials with Ángulo de flexión a 90° of 2.0 °/t | H22 | EN 573-3, EN 485 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip |
Coeficiente de dilatación térmica | 20 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | H22 | EN 573-3, EN 485 | |
100 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | H22 | EN 573-3, EN 485 | ||
Conductividad térmica | 225 W/(m·K) Show Material materials with Conductividad térmica of 225 W/(m·K) | H22 | EN 573-3, EN 485 | ||
20.0 °C | 215.0 W/(m·K) Show Material materials with Conductividad térmica of 215.0 W/(m·K) | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | |
Temperatura de fusión | 659.0 °C Show Material materials with Temperatura de fusión of 659.0 °C | H22 | EN 573-3, EN 485 |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 34500000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 34500000.0 - 35000000.0 S/m | H22 | EN 573-3, EN 485 | ||
20.0 °C | 36400000.0 - 37000000.0 S/m Show Material materials with Conductividad eléctrica of 36400000.0 - 37000000.0 S/m | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | |
Resistividad eléctrica | 2.86e-08 - 2.9e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.86e-08 - 2.9e-08 Ω·m | H22 | EN 573-3, EN 485 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 99.8 % Show Material materials with Aluminio of 99.8 % | H22 | EN 573-3, EN 485 | |
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Galio | 0.03 % Show Material materials with Galio of 0.03 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | H22 | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip |
0.15 % Show Material materials with Hierro of 0.15 % | H22 | EN 573-3, EN 485 | ||
Magnesio | 0.02 % Show Material materials with Magnesio of 0.02 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Manganeso | 0.02 % Show Material materials with Manganeso of 0.02 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Zinc | 0.06 % Show Material materials with Zinc of 0.06 % | H22 | DIN 1712-3, EN 573-3, EN 573-4, EN 485 | Sheet, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: very good, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good | |
Workability | Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H14) / very good (H12) |