DIN 1712-3 Grade 3.0255 H12

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

Pure aluminium This material is well anodically oxidizable, and possesses a good electrical and thermal conductivity. The splinter-giving workability is bad because of danger of smearing. Its mechanical strength is low, the plasticity high. The forming capacity and the chemical as well as the weather proofness are excellent. The material is well suitable for welding and braze welding. Application: apparatus engineering, roll bond, z-bond, household devices, camp and transportation containers for the chemical, pharmaceutical and food industry, roofings, linings, arts and crafts, packing, flow pressed parts (tubes, tube, doses, bottles), reflectors, generally metal-describe, large bottles (to 10 l), metal goods, far neck catches, heat exchanger (profiles, gilled pipes), pressure tanks according to AD-W 6/1, liquid air separation, thermal insulation, antennas, parabolic reflector, tank -, silo trucks, body parts, aircraft construction, tools, forms and devices in mechanical engineering.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM,AluKey.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueConditionRelated StandardsShape

Densidad

2.7 g/cm³

Show Material materials with Densidad of 2.7 g/cm³

H12

EN 573-3, EN 485

20.0 °C

2.7 g/cm³

Show Material materials with Densidad of 2.7 g/cm³

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Mecánica

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coeficiente de Poisson

0.33 [-]

Show Material materials with Coeficiente de Poisson of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Dureza Brinell

28.0 [-]

Show Material materials with Dureza Brinell of 28.0 [-]

H12

EN 573-3, EN 485

20.0 °C

30.0 [-]

Show Material materials with Dureza Brinell of 30.0 [-]

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Elongación

2.0 %

Show Material materials with Elongación of 2.0 %

H12

EN 573-3, EN 485

A50

4.0 %

Show Material materials with Elongación of 4.0 %

H12

EN 573-3, EN 485

A50

5.0 %

Show Material materials with Elongación of 5.0 %

H12

EN 573-3, EN 485

A50

7.0 %

Show Material materials with Elongación of 7.0 %

H12

EN 573-3, EN 485

A50

9.0 %

Show Material materials with Elongación of 9.0 %

H12

EN 573-3, EN 485

A50

9.0 %

Show Material materials with Elongación of 9.0 %

H12

EN 573-3, EN 485

A100

20.0 °C

6.0 %

Show Material materials with Elongación of 6.0 %

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

A10

20.0 °C

9.0 %

Show Material materials with Elongación of 9.0 %

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Módulo de cizallamiento

25.9 GPa

Show Material materials with Módulo de cizallamiento of 25.9 GPa

H12

EN 573-3, EN 485

20.0 °C

25.0 - 26.5 GPa

Show Material materials with Módulo de cizallamiento of 25.0 - 26.5 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Módulo elástico

-195.0 °C

78.4 GPa

Show Material materials with Módulo elástico of 78.4 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

-85.0 °C

73.5 GPa

Show Material materials with Módulo elástico of 73.5 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

-30.0 °C

71.4 GPa

Show Material materials with Módulo elástico of 71.4 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

69.0 GPa

Show Material materials with Módulo elástico of 69.0 GPa

H12

EN 573-3, EN 485

20.0 °C

60.0 - 70.0 GPa

Show Material materials with Módulo elástico of 60.0 - 70.0 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

20.0 °C

70.0 GPa

Show Material materials with Módulo elástico of 70.0 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

100.0 °C

68.6 GPa

Show Material materials with Módulo elástico of 68.6 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

150.0 °C

66.5 GPa

Show Material materials with Módulo elástico of 66.5 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

200.0 °C

63.0 GPa

Show Material materials with Módulo elástico of 63.0 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

250.0 °C

56.0 GPa

Show Material materials with Módulo elástico of 56.0 GPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 1000 Series Aluminium

Resistencia a la tracción

85.0 - 125.0 MPa

Show Material materials with Resistencia a la tracción of 85.0 - 125.0 MPa

H12

EN 573-3, EN 485

20.0 °C

90.0 - 130.0 MPa

Show Material materials with Resistencia a la tracción of 90.0 - 130.0 MPa

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Ángulo de flexión a 180°

0.5 °/t

Show Material materials with Ángulo de flexión a 180° of 0.5 °/t

H12

EN 573-3, EN 485

1.0 °/t

Show Material materials with Ángulo de flexión a 180° of 1.0 °/t

H12

EN 573-3, EN 485

Ángulo de flexión a 90°

0.5 °/t

Show Material materials with Ángulo de flexión a 90° of 0.5 °/t

H12

EN 573-3, EN 485

1.0 °/t

Show Material materials with Ángulo de flexión a 90° of 1.0 °/t

H12

EN 573-3, EN 485

2.0 °/t

Show Material materials with Ángulo de flexión a 90° of 2.0 °/t

H12

EN 573-3, EN 485

Aplicaciones térmicas

PropertyTemperatureValueConditionRelated StandardsShape

Calor específico

900.0 J/(kg·K)

Show Material materials with Calor específico of 900.0 J/(kg·K)

H12

EN 573-3, EN 485

20.0 °C

900.0 J/(kg·K)

Show Material materials with Calor específico of 900.0 J/(kg·K)

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Coeficiente de dilatación térmica

-50 °C

2.17e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.17e-05 1/K

H12

EN 573-3, EN 485, DIN 1712-3, EN 573-4

Sheet, Strip

-50.0 °C

2.17e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.17e-05 1/K

H12

EN 573-3, EN 485, DIN 1712-3, EN 573-4

Sheet, Strip

20 °C

2.17e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.17e-05 1/K

H12

EN 573-3, EN 485, DIN 1712-3, EN 573-4

Sheet, Strip

20 °C

2.35e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K

H12

EN 573-3, EN 485, DIN 1712-3, EN 573-4

Sheet, Strip

20 °C

2.4399999999999997e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.4399999999999997e-05 1/K

H12

EN 573-3, EN 485

20 °C

2.5399999999999997e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.5399999999999997e-05 1/K

H12

EN 573-3, EN 485

100 °C

2.35e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K

H12

EN 573-3, EN 485, DIN 1712-3, EN 573-4

Sheet, Strip

100.0 °C

2.35e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K

H12

EN 573-3, EN 485, DIN 1712-3, EN 573-4

Sheet, Strip

200 °C

2.4399999999999997e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.4399999999999997e-05 1/K

H12

EN 573-3, EN 485

200.0 °C

2.44e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.44e-05 1/K

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

300 °C

2.5399999999999997e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.5399999999999997e-05 1/K

H12

EN 573-3, EN 485

300.0 °C

2.54e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.54e-05 1/K

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Conductividad térmica

20.0 °C

210.0 - 220.0 W/(m·K)

Show Material materials with Conductividad térmica of 210.0 - 220.0 W/(m·K)

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Temperatura de fusión

646.0 - 657.0 °C

Show Material materials with Temperatura de fusión of 646.0 - 657.0 °C

H12

EN 573-3, EN 485

Eléctrico

PropertyTemperatureValueConditionRelated StandardsShape

Conductividad eléctrica

34000000.0 - 36000000.0 S/m

Show Material materials with Conductividad eléctrica of 34000000.0 - 36000000.0 S/m

H12

EN 573-3, EN 485

20.0 °C

34800000.0 - 36000000.0 S/m

Show Material materials with Conductividad eléctrica of 34800000.0 - 36000000.0 S/m

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Resistividad eléctrica

2.78e-08 - 2.94e-08 Ω·m

Show Material materials with Resistividad eléctrica of 2.78e-08 - 2.94e-08 Ω·m

H12

EN 573-3, EN 485

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminio

99.5 %

Show Material materials with Aluminio of 99.5 %

H12

EN 573-3, EN 485

Cobre

0.05 %

Show Material materials with Cobre of 0.05 %

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Hierro

0.4 %

Show Material materials with Hierro of 0.4 %

H12

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

0.40 %

Show Material materials with Hierro of 0.40 %

H12

EN 573-3, EN 485

Magnesio

0.05 %

Show Material materials with Magnesio of 0.05 %

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Manganeso

0.05 %

Show Material materials with Manganeso of 0.05 %

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Silicona

0.25 %

Show Material materials with Silicona of 0.25 %

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Titanio

0.05 %

Show Material materials with Titanio of 0.05 %

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Zinc

0.07 %

Show Material materials with Zinc of 0.07 %

H12

DIN 1712-3, EN 573-3, EN 573-4, EN 485

Sheet, Strip

Technological properties

Property
Anodizing

decorative: gut (EQ: sehr gut), Protective: very good

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Seawater: acceptable, weathering: good

Workability

Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H14) / very good (H12)