General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 g/cm³ Show Material materials with Densidad of 2.75 g/cm³ | Typical for Cast 1xx.x Series Aluminium |
Mecánica
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 1.8e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8e-05 - 2.4e-05 1/K | Typical for Cast 1xx.x Series Aluminium |
Conductividad térmica | 209.0 - 222.0 W/(m·K) Show Material materials with Conductividad térmica of 209.0 - 222.0 W/(m·K) | Typical for Cast 1xx.x Series Aluminium |
Temperatura de fusión | 643.0 - 657.0 °C Show Material materials with Temperatura de fusión of 643.0 - 657.0 °C | Typical for Cast 1xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 99.0 % Show Material materials with Aluminio of 99.0 % | Pink Sheets | Casting |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | Pink Sheets | Casting |
Hierro | 0.6 - 0.8 % Show Material materials with Hierro of 0.6 - 0.8 % | Pink Sheets | Casting |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % | Pink Sheets | Casting |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | Pink Sheets | Casting |