General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.8 g/cm³ Show Material materials with Densidad of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mecánica
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 875.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium |
Coeficiente de dilatación térmica | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium |
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Temperatura de fusión | 510.0 - 790.0 °C Show Material materials with Temperatura de fusión of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Cobre | 7.0 - 9.0 % Show Material materials with Cobre of 7.0 - 9.0 % | Pink Sheets | Casting |
Hierro | 0.40 % Show Material materials with Hierro of 0.40 % | Pink Sheets | Casting |
Magnesio | 5.6 - 6.5 % Show Material materials with Magnesio of 5.6 - 6.5 % | Pink Sheets | Casting |
Manganeso | 0.3 - 0.7 % Show Material materials with Manganeso of 0.3 - 0.7 % | Pink Sheets | Casting |
Níquel | 0.3 - 0.7 % Show Material materials with Níquel of 0.3 - 0.7 % | Pink Sheets | Casting |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | Pink Sheets | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | Pink Sheets | Casting |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | Pink Sheets | Casting |