General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.8 g/cm³ Show Material materials with Densidad of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | |||
Dureza Brinell | 105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T61 | Pink Sheets, ASTM B108 | Casting | ||
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | |||
Resistencia a la tracción | 220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
275.0 MPa Show Material materials with Resistencia a la tracción of 275.0 MPa | T61 | Pink Sheets, ASTM B108 | Casting |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 875.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium | |||
Coeficiente de dilatación térmica | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium | |||
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium | |||
Temperatura de fusión | 532.0 - 635.0 °C Show Material materials with Temperatura de fusión of 532.0 - 635.0 °C | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 3.5 - 4.5 % Show Material materials with Cobre of 3.5 - 4.5 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Hierro | 1.00 % Show Material materials with Hierro of 1.00 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Níquel | 1.7 - 2.3 % Show Material materials with Níquel of 1.7 - 2.3 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |