General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Dureza Brinell | 80.0 - 90.0 [-] Show Material materials with Dureza Brinell of 80.0 - 90.0 [-] | T61 | Pink Sheets, ASTM B108 | Casting | |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Resistencia a la tracción | 195.0 MPa Show Material materials with Resistencia a la tracción of 195.0 MPa | T61 | Pink Sheets, ASTM B108 | Casting | |
230.0 MPa Show Material materials with Resistencia a la tracción of 230.0 MPa | T61 | Pink Sheets, ASTM B108 | Casting | ||
245.0 MPa Show Material materials with Resistencia a la tracción of 245.0 MPa | T61 | Pink Sheets, ASTM B26 | Casting | ||
260.0 MPa Show Material materials with Resistencia a la tracción of 260.0 MPa | T61 | Pink Sheets, ASTM B108 | Casting |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | |||
Coeficiente de dilatación térmica | 1.6e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium | |||
Conductividad térmica | 130.0 - 180.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium | |||
Temperatura de fusión | 557.0 - 613.0 °C Show Material materials with Temperatura de fusión of 557.0 - 613.0 °C | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Hierro | 0.20 % Show Material materials with Hierro of 0.20 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Magnesio | 0.25 - 0.45 % Show Material materials with Magnesio of 0.25 - 0.45 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Silicona | 6.5 - 7.5 % Show Material materials with Silicona of 6.5 - 7.5 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T61 | Pink Sheets, ASTM B108, ASTM B26 | Casting |