General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Resistencia a la tracción | 280.0 MPa Show Material materials with Resistencia a la tracción of 280.0 MPa | F | Pink Sheets, ASTM B85 | Casting |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | |||
Coeficiente de dilatación térmica | 1.6e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium | |||
Conductividad térmica | 130.0 - 180.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium | |||
Temperatura de fusión | 507.0 - 649.0 °C Show Material materials with Temperatura de fusión of 507.0 - 649.0 °C | F | Pink Sheets, ASTM B85 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 4.0 - 5.0 % Show Material materials with Cobre of 4.0 - 5.0 % | F | Pink Sheets, ASTM B85 | Casting |
Hierro | 1.30 % Show Material materials with Hierro of 1.30 % | F | Pink Sheets, ASTM B85 | Casting |
Magnesio | 0.45 - 0.65 % Show Material materials with Magnesio of 0.45 - 0.65 % | F | Pink Sheets, ASTM B85 | Casting |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | F | Pink Sheets, ASTM B85 | Casting |
Silicona | 16.0 - 18.0 % Show Material materials with Silicona of 16.0 - 18.0 % | F | Pink Sheets, ASTM B85 | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | F | Pink Sheets, ASTM B85 | Casting |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | F | Pink Sheets, ASTM B85 | Casting |