General
Property | Value | Comment |
---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | Typical for Cast 8xx.x Series Aluminium |
Mecánica
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 8xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | Typical for Cast 8xx.x Series Aluminium |
Temperatura de fusión | 205.0 - 650.0 °C Show Material materials with Temperatura de fusión of 205.0 - 650.0 °C | Typical for Cast 8xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Cobre | 1.7 - 2.3 % Show Material materials with Cobre of 1.7 - 2.3 % | Pink Sheets | Casting |
Estaño | 5.5 - 7.0 % Show Material materials with Estaño of 5.5 - 7.0 % | Pink Sheets | Casting |
Hierro | 0.50 % Show Material materials with Hierro of 0.50 % | Pink Sheets | Casting |
Magnesio | 0.7 - 0.9 % Show Material materials with Magnesio of 0.7 - 0.9 % | Pink Sheets | Casting |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | Pink Sheets | Casting |
Níquel | 0.9 - 1.5 % Show Material materials with Níquel of 0.9 - 1.5 % | Pink Sheets | Casting |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | Pink Sheets | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | Pink Sheets | Casting |