Chemical properties
Property | Value | Related Standards |
---|---|---|
Berilio | 4.5 - 6.0 % Show Material materials with Berilio of 4.5 - 6.0 % | Gold Sheets |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | Gold Sheets |
Cromo | 0.02 % Show Material materials with Cromo of 0.02 % | Gold Sheets |
Hierro | 0.40 % Show Material materials with Hierro of 0.40 % | Gold Sheets |
Magnesio | 0.5 % Show Material materials with Magnesio of 0.5 % | Gold Sheets |
Manganeso | 0.02 % Show Material materials with Manganeso of 0.02 % | Gold Sheets |
Níquel | 0.02 % Show Material materials with Níquel of 0.02 % | Gold Sheets |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | Gold Sheets |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % | Gold Sheets |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | Gold Sheets |