Chemical properties
Property | Value | Related Standards |
---|---|---|
Calcio | 0.5 % Show Material materials with Calcio of 0.5 % | Gold Sheets |
Circonio | 0.1 % Show Material materials with Circonio of 0.1 % | Gold Sheets |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | Gold Sheets |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % | Gold Sheets |
Estroncio | 9.0 - 11.0 % Show Material materials with Estroncio of 9.0 - 11.0 % | Gold Sheets |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % | Gold Sheets |
Hierro | 1.50 % Show Material materials with Hierro of 1.50 % | Gold Sheets |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | Gold Sheets |
Níquel | 0.05 % Show Material materials with Níquel of 0.05 % | Gold Sheets |
Silicona | 12.0 - 16.0 % Show Material materials with Silicona of 12.0 - 16.0 % | Gold Sheets |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | Gold Sheets |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % | Gold Sheets |