Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze |
Dureza Brinell | 23.0 °C | 241 [-] Show Material materials with Dureza Brinell of 241 [-] | |
Módulo elástico | 23.0 °C | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 12 - 13.5 % Show Material materials with Aluminio of 12 - 13.5 % |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | Rest Cu |