Acero bajo en carbono
EN 10028-3 Grade P275NH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10149-3 Grade S260NC normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10149-2 Grade S315MC thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10149-2 Grade S355MC thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10149-3 Grade S315NC normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Unclassified Carbon Steel
ASTM A516 Grade 380 As-Rolled or Normalized and/or Stress RelievedSuministrada por:
1 proveedor Matmatch
Acero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedWrought Copper Bronze Aluminium Bronze
NC4 - CuAl10Ni5Fe4 - C63000 / C63200Suministrada por:
Lebronze AlloysAcero inoxidable ferrítico
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Acero de alto carbono
EN 10250-2 Grade C60 normalized and tempered (+NT)Acero inoxidable martensítico
SEW 400 Grade X4CrNi13-4 quenched and tempered (+QT1)Wrought Copper Nickel Grade
HARDIALL® - TS 120 U - CuNi15Sn8 - C72900Suministrada por:
Lebronze AlloysAcero inoxidable ferrítico
EN 10088-1 Grade X2CrNi12 quenched and tempered (+QT)Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 TH