Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze |
Dureza Brinell | 23.0 °C | 170 - 185 [-] Show Material materials with Dureza Brinell of 170 - 185 [-] | |
Elongación | 23.0 °C | 5 % Show Material materials with Elongación of 5 % | |
Límite elástico Rp 0,2 | 23.0 °C | 320 - 380 MPa Show Material materials with Límite elástico Rp 0,2 of 320 - 380 MPa | |
Módulo elástico | 23.0 °C | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze |
Resistencia a la tracción | 23.0 °C | 680 - 750 MPa Show Material materials with Resistencia a la tracción of 680 - 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 10 - 12 % Show Material materials with Aluminio of 10 - 12 % |
Cobre | 72 - 78 % Show Material materials with Cobre of 72 - 78 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 4 - 7 % Show Material materials with Hierro of 4 - 7 % |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % |
Manganeso | 2.5 % Show Material materials with Manganeso of 2.5 % |
Níquel | 4 - 7.5 % Show Material materials with Níquel of 4 - 7.5 % |
Otro | for Mould cast (Ingot metals and Castings): Fe > 3.0. Al > 9.0. Cu < 84.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |