Chemical properties
Property | Value |
---|---|
Antimonio | 4E-4 % Show Material materials with Antimonio of 4E-4 % |
Arsénico | 5E-4 % Show Material materials with Arsénico of 5E-4 % |
Azufre | 1.5E-3 % Show Material materials with Azufre of 1.5E-3 % |
Bismuto | 2E-4 % Show Material materials with Bismuto of 2E-4 % |
Cadmio | 1E-4 % Show Material materials with Cadmio of 1E-4 % |
Cobre | 99.99 % Show Material materials with Cobre of 99.99 % |
Estaño | 2E-4 % Show Material materials with Estaño of 2E-4 % |
Fósforo | 3E-4 - 6E-3 % Show Material materials with Fósforo of 3E-4 - 6E-3 % |
Hierro | 1E-3 % Show Material materials with Hierro of 1E-3 % |
Manganeso | 5E-4 % Show Material materials with Manganeso of 5E-4 % |
Níquel | 1E-3 % Show Material materials with Níquel of 1E-3 % |
Otro | total 0.03. excluded Ag, P |
Plata | 2.5E-3 % Show Material materials with Plata of 2.5E-3 % |
Plomo | 5E-4 % Show Material materials with Plomo of 5E-4 % |
Telurio | 2E-4 % Show Material materials with Telurio of 2E-4 % |
Zinc | 1E-4 % Show Material materials with Zinc of 1E-4 % |