General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Elongación | 23.0 °C | 30 % Show Material materials with Elongación of 30 % | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 126.5 GPa Show Material materials with Módulo elástico of 126.5 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 20.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | |
100.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
Conductividad térmica | 23.0 °C | 380 W/(m·K) Show Material materials with Conductividad térmica of 380 W/(m·K) | |
Temperatura de fusión | 1082 °C Show Material materials with Temperatura de fusión of 1082 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.40E+7 - 5.70E+7 S/m Show Material materials with Conductividad eléctrica of 5.40E+7 - 5.70E+7 S/m |
Resistividad eléctrica | 23.0 °C | 1.75E-8 - 1.85E-8 Ω·m Show Material materials with Resistividad eléctrica of 1.75E-8 - 1.85E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Bismuto | 5E-4 % Show Material materials with Bismuto of 5E-4 % |
Fósforo | 1E-3 - 7E-3 % Show Material materials with Fósforo of 1E-3 - 7E-3 % |
Otro | total 0.0065. excluded Ag, O |
Plata | 0.08 - 0.12 % Show Material materials with Plata of 0.08 - 0.12 % |