General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Dureza Brinell | 23.0 °C | 90 [-] Show Material materials with Dureza Brinell of 90 [-] | |
Dureza Vickers | 23.0 °C | 90 [-] Show Material materials with Dureza Vickers of 90 [-] | |
Elongación | 23.0 °C | 7 % Show Material materials with Elongación of 7 % | |
Elongation A100 | 23.0 °C | 3 % Show Material materials with Elongation A100 of 3 % | |
Límite elástico Rp 0,2 | 23.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa | |
Resistencia a la tracción | 23.0 °C | 250 MPa Show Material materials with Resistencia a la tracción of 250 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 20.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | |
100.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | ||
Conductividad térmica | 23.0 °C | 370 - 375 W/(m·K) Show Material materials with Conductividad térmica of 370 - 375 W/(m·K) | |
Temperatura de fusión | 1067 - 1079 °C Show Material materials with Temperatura de fusión of 1067 - 1079 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.40E+7 - 5.50E+7 S/m Show Material materials with Conductividad eléctrica of 5.40E+7 - 5.50E+7 S/m |
Resistividad eléctrica | 23.0 °C | 1.82E-8 - 1.85E-8 Ω·m Show Material materials with Resistividad eléctrica of 1.82E-8 - 1.85E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.2 - 0.7 % Show Material materials with Azufre of 0.2 - 0.7 % |
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Otro | Rest Cu, total 0.1 |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : very good to good, soft brazing: very good | |
Workability | Cold forming degree between anneals: max. 70 %, general (condition): good |