General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 85 - 115 [-] Show Material materials with Dureza Vickers of 85 - 115 [-] |
Elongación | 20.0 °C | 50 % Show Material materials with Elongación of 50 % |
Elongation A100 | 20.0 °C | 40 % Show Material materials with Elongation A100 of 40 % |
Límite elástico Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa |
Resistencia a la tracción | 20.0 °C | 260 - 380 MPa Show Material materials with Resistencia a la tracción of 260 - 380 MPa |
Chemical properties
Property | Value |
---|---|
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % |
Otro | Rest Cu, total 0.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.8 - 2 % Show Material materials with Silicona of 0.8 - 2 % |
Zinc | 1.5 % Show Material materials with Zinc of 1.5 % |