General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 85 - 115 [-] Show Material materials with Dureza Brinell of 85 - 115 [-] |
Dureza Vickers | 20.0 °C | 90 - 120 [-] Show Material materials with Dureza Vickers of 90 - 120 [-] |
Elongación | 20.0 °C | 50 % Show Material materials with Elongación of 50 % |
Elongation A100 | 20.0 °C | 40 % Show Material materials with Elongation A100 of 40 % |
Límite elástico Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Límite elástico Rp 0,2 of 260 MPa |
Módulo elástico | 20.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa |
Resistencia a la tracción | 20.0 °C | 380 MPa Show Material materials with Resistencia a la tracción of 380 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K |
100.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | |
Conductividad térmica | 20.0 °C | 38 W/(m·K) Show Material materials with Conductividad térmica of 38 W/(m·K) |
Temperatura de fusión | 970 - 1025 °C Show Material materials with Temperatura de fusión of 970 - 1025 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 3.80E+6 - 4.00E+6 S/m Show Material materials with Conductividad eléctrica of 3.80E+6 - 4.00E+6 S/m |
Resistividad eléctrica | 20.0 °C | 2.5E-7 - 2.63E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.5E-7 - 2.63E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.7 - 1.3 % Show Material materials with Manganeso of 0.7 - 1.3 % |
Otro | Rest Cu, total 0.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 2.7 - 3.2 % Show Material materials with Silicona of 2.7 - 3.2 % |
Zinc | 0.4 % Show Material materials with Zinc of 0.4 % |