General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 40 - 60 [-] Show Material materials with Dureza Brinell of 40 - 60 [-] |
Dureza Vickers | 20.0 °C | 40 - 65 [-] Show Material materials with Dureza Vickers of 40 - 65 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 40 MPa Show Material materials with Límite elástico Rp 0,2 of 40 MPa |
Módulo elástico | 20.0 °C | 135 GPa Show Material materials with Módulo elástico of 135 GPa |
Resistencia a la tracción | 20.0 °C | 180 MPa Show Material materials with Resistencia a la tracción of 180 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K |
100.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | |
Conductividad térmica | 20.0 °C | 167 - 330 W/(m·K) Show Material materials with Conductividad térmica of 167 - 330 W/(m·K) |
Temperatura de fusión | 1073 - 1080 °C Show Material materials with Temperatura de fusión of 1073 - 1080 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.60E+7 - 5.40E+7 S/m Show Material materials with Conductividad eléctrica of 2.60E+7 - 5.40E+7 S/m |
Resistividad eléctrica | 20.0 °C | 1.85E-8 - 3.85E-8 Ω·m Show Material materials with Resistividad eléctrica of 1.85E-8 - 3.85E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Circonio | 0.1 - 0.2 % Show Material materials with Circonio of 0.1 - 0.2 % |
Otro | Rest Cu, total 0.1 |