General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.4 g/cm³ Show Material materials with Densidad of 7.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 190 - 235 [-] Show Material materials with Dureza Brinell of 190 - 235 [-] |
Dureza Vickers | 20.0 °C | 200 - 245 [-] Show Material materials with Dureza Vickers of 200 - 245 [-] |
Elongación | 20.0 °C | 10 % Show Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 20.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa |
Resistencia a la tracción | 20.0 °C | 750 MPa Show Material materials with Resistencia a la tracción of 750 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 10.5 - 12.5 % Show Material materials with Aluminio of 10.5 - 12.5 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 5 - 7 % Show Material materials with Hierro of 5 - 7 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 5 - 7 % Show Material materials with Níquel of 5 - 7 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |