Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 543 - 643 °C Show Material materials with Temperatura de fusión of 543 - 643 °C |
General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.84 g/cm³ Show Material materials with Densidad of 2.84 g/cm³ |
Chemical properties
Property | Value |
---|---|
Circonio | 0.25 % Show Material materials with Circonio of 0.25 % |
Cobre | 6.8 % Show Material materials with Cobre of 6.8 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Magnesio | 0.02 % Show Material materials with Magnesio of 0.02 % |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Vanadio | 0.15 % Show Material materials with Vanadio of 0.15 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |