General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 55 - 85 [-] Show Material materials with Dureza Vickers of 55 - 85 [-] |
Elongación | 20.0 °C | 45 % Show Material materials with Elongación of 45 % |
Elongación A50 | 20.0 °C | 36 % Show Material materials with Elongación A50 of 36 % |
Límite elástico Rp 0,2 | 20.0 °C | 140 - 170 MPa Show Material materials with Límite elástico Rp 0,2 of 140 - 170 MPa |
Módulo elástico | 20.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa |
Resistencia a la tracción | 20.0 °C | 260 - 310 MPa Show Material materials with Resistencia a la tracción of 260 - 310 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) |
Coeficiente de dilatación térmica | 20.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K |
100.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | |
Conductividad térmica | 20.0 °C | 159 W/(m·K) Show Material materials with Conductividad térmica of 159 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.20E+7 S/m Show Material materials with Conductividad eléctrica of 2.20E+7 S/m |
Resistividad eléctrica | 20.0 °C | 4.55E-8 Ω·m Show Material materials with Resistividad eléctrica of 4.55E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobre | 84 - 86 % Show Material materials with Cobre of 84 - 86 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Zn, total 0.1 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Technological properties
Property | ||
---|---|---|
Brazing | soft brazing: very good | |
Workability | general (condition): good |