General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser,Wanddicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 70 - 110 [-] Show Material materials with Dureza Brinell of 70 - 110 [-] |
Dureza Vickers | 20.0 °C | 70 - 110 [-] Show Material materials with Dureza Vickers of 70 - 110 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa |
Resistencia a la tracción | 20.0 °C | 280 MPa Show Material materials with Resistencia a la tracción of 280 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Arsénico | 0.02 - 0.15 % Show Material materials with Arsénico of 0.02 - 0.15 % |
Cobre | 61.5 - 63.5 % Show Material materials with Cobre of 61.5 - 63.5 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % |