General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.5 g/cm³ Show Material materials with Densidad of 8.5 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Wanddicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 75 - 105 [-] Show Material materials with Dureza Vickers of 75 - 105 [-] |
Elongación | 20.0 °C | 45 % Show Material materials with Elongación of 45 % |
Límite elástico Rp 0,2 | 20.0 °C | 130 MPa Show Material materials with Límite elástico Rp 0,2 of 130 MPa |
Resistencia a la tracción | 20.0 °C | 340 MPa Show Material materials with Resistencia a la tracción of 340 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Arsénico | 0.02 - 0.06 % Show Material materials with Arsénico of 0.02 - 0.06 % |
Cobre | 69 - 71 % Show Material materials with Cobre of 69 - 71 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.07 % Show Material materials with Plomo of 0.07 % |