General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Dureza Brinell of 120 - 150 [-] |
Dureza Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Dureza Vickers of 125 - 155 [-] |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 300 MPa Show Material materials with Límite elástico Rp 0,2 of 300 MPa |
Resistencia a la tracción | 20.0 °C | 490 MPa Show Material materials with Resistencia a la tracción of 490 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 1.3 % Show Material materials with Aluminio of 0.3 - 1.3 % |
Cobre | 58 - 60 % Show Material materials with Cobre of 58 - 60 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 1.5 - 2.5 % Show Material materials with Manganeso of 1.5 - 2.5 % |
Níquel | 2 - 3 % Show Material materials with Níquel of 2 - 3 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.2 - 0.8 % Show Material materials with Plomo of 0.2 - 0.8 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |