General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.77 g/cm³ Show Material materials with Densidad of 2.77 g/cm³ | T62 | WL 3.1354 | Strip, Sheet, Plate |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Dureza Brinell | 120.0 [-] Show Material materials with Dureza Brinell of 120.0 [-] | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Módulo de cizallamiento | 27.6 GPa Show Material materials with Módulo de cizallamiento of 27.6 GPa | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Módulo elástico | 72.4 GPa Show Material materials with Módulo elástico of 72.4 GPa | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Resistencia a la tracción | 415.0 MPa Show Material materials with Resistencia a la tracción of 415.0 MPa | T62 | WL 3.1354 | Strip, Sheet, Plate | |
435.0 MPa Show Material materials with Resistencia a la tracción of 435.0 MPa | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
440.0 MPa Show Material materials with Resistencia a la tracción of 440.0 MPa | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
Ángulo de flexión a 180° | 4.0 °/t Show Material materials with Ángulo de flexión a 180° of 4.0 °/t | T62 | WL 3.1354 | Strip, Sheet, Plate |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.1499999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1499999999999997e-05 1/K | T62 | WL 3.1354 | Strip, Sheet, Plate | |
100 °C | 2.1499999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1499999999999997e-05 1/K | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
Conductividad térmica | 109.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 109.0 - 160.0 W/(m·K) | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
Temperatura de fusión | 500.0 - 640.0 °C Show Material materials with Temperatura de fusión of 500.0 - 640.0 °C | T62 | WL 3.1354 | Strip, Sheet, Plate |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 15000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 15000000.0 - 23000000.0 S/m | T62 | WL 3.1354 | Strip, Sheet, Plate |
Resistividad eléctrica | 4.35e-08 - 6.67e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.35e-08 - 6.67e-08 Ω·m | T62 | WL 3.1354 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 3.8 - 4.9 % Show Material materials with Cobre of 3.8 - 4.9 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Hierro | 0.50 % Show Material materials with Hierro of 0.50 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Manganeso | 0.3 - 0.9 % Show Material materials with Manganeso of 0.3 - 0.9 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |