General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.71 g/cm³ Show Supplier Material materials with Densidad of 8.71 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 210 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 210 [-] | HBW 10/3000 |
Dureza Rockwell B | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Rockwell B of 95 [-] | |
Elongación A5 | 23.0 °C | 11 % Show Supplier Material materials with Elongación A5 of 11 % | |
Estricción | 23.0 °C | 20 % Show Supplier Material materials with Estricción of 20 % | |
Límite elástico Rp0.5 | 23.0 °C | 496 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 496 MPa | |
Límite elástico a la compresión, 0,1% | 23.0 °C | 552 MPa Show Supplier Material materials with Límite elástico a la compresión, 0,1% of 552 MPa | |
Módulo elástico | 23.0 °C | 131 GPa Show Supplier Material materials with Módulo elástico of 131 GPa | |
Resistencia a la tracción | 23.0 °C | 648 MPa Show Supplier Material materials with Resistencia a la tracción of 648 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Supplier Material materials with Calor específico of 380 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 208 W/(m·K) Show Supplier Material materials with Conductividad térmica of 208 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.80E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.80E+7 S/m |
Specific Electrical conductivity | 48 % IACS Show Supplier Material materials with Specific Electrical conductivity of 48 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | AMPCOLOY® 940 is used wherever a good electrical or thermal conductivity is required together with high mechanical properties: Electrode holders and seam welding shafts, Spot welding electrodes, seam welding discs, projection and butt welding dies, principally for stainless steel and Monel, Plunger tips for cold chamber aluminium high pressure die casting machines and moulds for low pressure die casting machines, Parts of moulds for injection moulding of plastics, injection-nozzles and cooling pins, Chill moulds for casting brass and certain bronzes, Brake drums for paper winding rolls, Warm pressed parts for energy engineering. |