General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 140 [-] Show Supplier Material materials with Dureza Brinell of 140 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % | in 2″ (51 mm) |
Resistencia a la tracción | 23.0 °C | 530 MPa Show Supplier Material materials with Resistencia a la tracción of 530 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 7.5 - 9.5 % Show Supplier Material materials with Aluminio of 7.5 - 9.5 % | ||
Cobre | Balance, including silver | ||
Hierro | 1.5 - 2.5 % Show Supplier Material materials with Hierro of 1.5 - 2.5 % | ||
Manganeso | 1 - 2.5 % Show Supplier Material materials with Manganeso of 1 - 2.5 % | ||
Níquel | 1.8 - 3 % Show Supplier Material materials with Níquel of 1.8 - 3 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Ship propellers,Bearing overlays,Pumps,Chemical industry,Breaker blocks,Guide grooves |