General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.71 g/cm³ Show Supplier Material materials with Densidad of 8.71 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 210 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 210 [-] | HBW 10/3000 |
Dureza Rockwell B | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Rockwell B of 95 [-] | |
Elongación A5 | 23.0 °C | 8 % Show Supplier Material materials with Elongación A5 of 8 % | |
Estricción | 23.0 °C | 18 % Show Supplier Material materials with Estricción of 18 % | |
Límite elástico Rp0.5 | 23.0 °C | 475 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 475 MPa | |
Módulo elástico | 23.0 °C | 131 GPa Show Supplier Material materials with Módulo elástico of 131 GPa | |
Resistencia a la tracción | 23.0 °C | 544 MPa Show Supplier Material materials with Resistencia a la tracción of 544 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Supplier Material materials with Calor específico of 380 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 208 W/(m·K) Show Supplier Material materials with Conductividad térmica of 208 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.80E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.80E+7 S/m |
Specific Electrical conductivity | 48 % IACS Show Supplier Material materials with Specific Electrical conductivity of 48 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | AMPCOLOY® 940 is used wherever a good electrical or thermal conductivity is required together with high mechanical properties: Electrode holders, parts for energy engineering |