General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 125 - 152 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 125 - 152 [-] | HBW 10/1000 |
Dureza Rockwell B | 23.0 °C | 72 - 82 [-] Show Supplier Material materials with Dureza Rockwell B of 72 - 82 [-] | |
Elongación A5 | 23.0 °C | 18 - 20 % Show Supplier Material materials with Elongación A5 of 18 - 20 % | |
Límite elástico Rp0.5 | 23.0 °C | 410 - 466 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 410 - 466 MPa | |
Módulo elástico | 23.0 °C | 120 GPa Show Supplier Material materials with Módulo elástico of 120 GPa | |
Resistencia a la tracción | 23.0 °C | 465 - 520 MPa Show Supplier Material materials with Resistencia a la tracción of 465 - 520 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Supplier Material materials with Calor específico of 380 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K |
Conductividad térmica | 23.0 °C | 320 W/(m·K) Show Supplier Material materials with Conductividad térmica of 320 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.10E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 5.10E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Supplier Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Resistance welding tips; Electrode caps for the automotive industry; Tong arms for welding robots; Electrode holders; Parts for the energy engineering; Press parts |