General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.95 g/cm³ Show Supplier Material materials with Densidad of 7.95 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 140 - 153 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 140 - 153 [-] | HBW 10/3000 |
Dureza Rockwell B | 23.0 °C | 78 - 82 [-] Show Supplier Material materials with Dureza Rockwell B of 78 - 82 [-] | |
Elongación A5 | 23.0 °C | 40 - 42 % Show Supplier Material materials with Elongación A5 of 40 - 42 % | |
Energía de impacto Charpy | 23.0 °C | 54 - 61 J Show Supplier Material materials with Energía de impacto Charpy of 54 - 61 J | |
Energía de impacto Izod | 23.0 °C | 81 - 88 J Show Supplier Material materials with Energía de impacto Izod of 81 - 88 J | |
Estricción | 23.0 °C | 35 - 40 % Show Supplier Material materials with Estricción of 35 - 40 % | |
Límite elástico Rp0.5 | 23.0 °C | 214 - 283 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 214 - 283 MPa | |
Límite elástico a la compresión, 0,1% | 23.0 °C | 248 MPa Show Supplier Material materials with Límite elástico a la compresión, 0,1% of 248 MPa | |
Límite proporcional en compresión | 23.0 °C | 145 - 172 MPa Show Supplier Material materials with Límite proporcional en compresión of 145 - 172 MPa | |
Módulo elástico | 23.0 °C | 124 GPa Show Supplier Material materials with Módulo elástico of 124 GPa | |
Resistencia a la compresión | 23.0 °C | 689 - 862 MPa Show Supplier Material materials with Resistencia a la compresión of 689 - 862 MPa | |
Resistencia a la fatiga | 23.0 °C | 145 - 179 MPa Show Supplier Material materials with Resistencia a la fatiga of 145 - 179 MPa | 100.000.000 cycles |
Resistencia a la tracción | 23.0 °C | 483 - 552 MPa Show Supplier Material materials with Resistencia a la tracción of 483 - 552 MPa | |
Resistencia al cizallamiento | 23.0 °C | 290 - 359 MPa Show Supplier Material materials with Resistencia al cizallamiento of 290 - 359 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Calor específico of 420 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.63E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.63E-5 1/K |
Conductividad térmica | 23.0 °C | 54 W/(m·K) Show Supplier Material materials with Conductividad térmica of 54 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 7.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 7.00E+6 S/m |
Specific Electrical conductivity | 12 % IACS Show Supplier Material materials with Specific Electrical conductivity of 12 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | AMPCO® 8 sheet and plate has excellent corrosion resistance, not only in alkaline or reducing environments but also in oxydising media. This alloy is ideally suited for applications in the chemical and marine industry. Its inherent wear resistance properties make it well adopted for wear strips and wear plates. Other uses, where both corrosion and wear are factors include chutes, troughs and wear plates in contact with both dry and wet abrasive cereals and crystalline chemicals, etc. |