General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.45 g/cm³ Show Supplier Material materials with Densidad of 7.45 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 207 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 207 [-] | HBW 10/3000 |
Dureza Rockwell B | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Rockwell B of 95 [-] | |
Elongación A5 | 23.0 °C | 16 % Show Supplier Material materials with Elongación A5 of 16 % | |
Energía de impacto Charpy | 23.0 °C | 16.3 J Show Supplier Material materials with Energía de impacto Charpy of 16.3 J | |
Energía de impacto Izod | 23.0 °C | 24 J Show Supplier Material materials with Energía de impacto Izod of 24 J | |
Estricción | 23.0 °C | 16 % Show Supplier Material materials with Estricción of 16 % | |
Límite elástico Rp0.5 | 23.0 °C | 386 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 386 MPa | |
Límite elástico a la compresión, 0,1% | 23.0 °C | 345 MPa Show Supplier Material materials with Límite elástico a la compresión, 0,1% of 345 MPa | |
Límite proporcional | 23.0 °C | 214 MPa Show Supplier Material materials with Límite proporcional of 214 MPa | |
Límite proporcional en compresión | 23.0 °C | 310 MPa Show Supplier Material materials with Límite proporcional en compresión of 310 MPa | |
Módulo elástico | 23.0 °C | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa | |
Resistencia a la compresión | 23.0 °C | 1034 MPa Show Supplier Material materials with Resistencia a la compresión of 1034 MPa | |
Resistencia a la fatiga | 23.0 °C | 248 MPa Show Supplier Material materials with Resistencia a la fatiga of 248 MPa | 100.000.000 cycles |
Resistencia a la tracción | 23.0 °C | 758 MPa Show Supplier Material materials with Resistencia a la tracción of 758 MPa | |
Resistencia al cizallamiento | 23.0 °C | 421 MPa Show Supplier Material materials with Resistencia al cizallamiento of 421 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Calor específico of 420 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K |
Conductividad térmica | 23.0 °C | 59 W/(m·K) Show Supplier Material materials with Conductividad térmica of 59 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 7.50E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 7.50E+6 S/m |
Specific Electrical conductivity | 13 % IACS Show Supplier Material materials with Specific Electrical conductivity of 13 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | AMPCO® 18.23 gives a successful performance under heavy loads and impact conditions and makes it a preferred material for heavy-duty worm gears and similar applications. |