General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.53 g/cm³ Show Supplier Material materials with Densidad of 7.53 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 212 - 228 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 212 - 228 [-] | HBW 10/3000 |
Dureza Rockwell B | 23.0 °C | 96 - 98 [-] Show Supplier Material materials with Dureza Rockwell B of 96 - 98 [-] | |
Elongación A5 | 23.0 °C | 15 - 20 % Show Supplier Material materials with Elongación A5 of 15 - 20 % | |
Energía de impacto Charpy | 23.0 °C | 11.3 J Show Supplier Material materials with Energía de impacto Charpy of 11.3 J | |
Energía de impacto Izod | 23.0 °C | 13.6 J Show Supplier Material materials with Energía de impacto Izod of 13.6 J | |
Estricción | 23.0 °C | 15 - 20 % Show Supplier Material materials with Estricción of 15 - 20 % | |
Límite elástico Rp0.5 | 23.0 °C | 420 - 517 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 420 - 517 MPa | |
Límite elástico a la compresión, 0,1% | 23.0 °C | 303 MPa Show Supplier Material materials with Límite elástico a la compresión, 0,1% of 303 MPa | |
Límite proporcional en compresión | 23.0 °C | 262 - 276 MPa Show Supplier Material materials with Límite proporcional en compresión of 262 - 276 MPa | |
Módulo elástico | 23.0 °C | 117 GPa Show Supplier Material materials with Módulo elástico of 117 GPa | |
Resistencia a la compresión | 23.0 °C | 965 - 1034 MPa Show Supplier Material materials with Resistencia a la compresión of 965 - 1034 MPa | |
Resistencia a la fatiga | 23.0 °C | 255 - 262 MPa Show Supplier Material materials with Resistencia a la fatiga of 255 - 262 MPa | 100.000.000 cycles |
Resistencia a la tracción | 23.0 °C | 772 - 814 MPa Show Supplier Material materials with Resistencia a la tracción of 772 - 814 MPa | |
Resistencia al cizallamiento | 23.0 °C | 448 - 483 MPa Show Supplier Material materials with Resistencia al cizallamiento of 448 - 483 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Calor específico of 450 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K |
Conductividad térmica | 23.0 °C | 46 W/(m·K) Show Supplier Material materials with Conductividad térmica of 46 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Specific Electrical conductivity | 9 % IACS Show Supplier Material materials with Specific Electrical conductivity of 9 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 10 % Show Supplier Material materials with Aluminio of 10 % |
Cobre | Balance |
Hierro | 2.5 % Show Supplier Material materials with Hierro of 2.5 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Níquel | 5 % Show Supplier Material materials with Níquel of 5 % |
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | AMPCO® 45 is recommended for heavy-duty high-loaded mechanical and corrosive applications. Typical applications involving abrasive wear, friction, deformation, chemical erosion include: Aircraft bearings/bushings, Pump, marine shafts and wear rings, Valve spindles and seats, Machine tool parts. The spark-resistance properties make it suitable for safety tools and machine tool components in explosive environments. |