General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.45 g/cm³ Show Supplier Material materials with Densidad of 7.45 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 286 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 286 [-] | HBW 10/3000 |
Dureza Rockwell C | 23.0 °C | 29 [-] Show Supplier Material materials with Dureza Rockwell C of 29 [-] | |
Elongación A5 | 23.0 °C | 8 % Show Supplier Material materials with Elongación A5 of 8 % | |
Energía de impacto Charpy | 23.0 °C | 7 J Show Supplier Material materials with Energía de impacto Charpy of 7 J | |
Estricción | 23.0 °C | 12 - 13 % Show Supplier Material materials with Estricción of 12 - 13 % | |
Límite elástico Rp0.5 | 23.0 °C | 724 - 793 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 724 - 793 MPa | |
Límite elástico a la compresión, 0,1% | 23.0 °C | 689 - 731 MPa Show Supplier Material materials with Límite elástico a la compresión, 0,1% of 689 - 731 MPa | |
Módulo elástico | 23.0 °C | 124 GPa Show Supplier Material materials with Módulo elástico of 124 GPa | |
Resistencia a la compresión | 23.0 °C | 1324 MPa Show Supplier Material materials with Resistencia a la compresión of 1324 MPa | |
Resistencia a la fatiga | 23.0 °C | 352 MPa Show Supplier Material materials with Resistencia a la fatiga of 352 MPa | 100.000.000 cycles |
Resistencia a la tracción | 23.0 °C | 965 - 1000 MPa Show Supplier Material materials with Resistencia a la tracción of 965 - 1000 MPa | |
Resistencia al cizallamiento | 23.0 °C | 538 MPa Show Supplier Material materials with Resistencia al cizallamiento of 538 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Calor específico of 450 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
Conductividad térmica | 23.0 °C | 42 W/(m·K) Show Supplier Material materials with Conductividad térmica of 42 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 4.80E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 4.80E+6 S/m |
Specific Electrical conductivity | 8.2 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8.2 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 10.5 % Show Supplier Material materials with Aluminio of 10.5 % |
Cobre | Balance |
Hierro | 4.8 % Show Supplier Material materials with Hierro of 4.8 % |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % |
Níquel | 5 % Show Supplier Material materials with Níquel of 5 % |
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | AMPCO® M4 was initially developed as an aircraft specification alloy for gears in retractable landing assemblies, engine spacer bearings and other similar applications. It is rapidly growing in use where higher mechanical properties at elevated temperatures together with corrosion-resistant properties are required. Typical applications include aircraft landing gear bearings and bushings, bending dies (shoes and mandrels) for the tube bending industry, gear wheels and wear/guide plates, etc.. |