General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 125 [-] Show Supplier Material materials with Dureza Brinell of 125 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 47 % Show Supplier Material materials with Elongación of 47 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 53 % Show Supplier Material materials with Estricción of 53 % | |
Límite elástico | 23.0 °C | 193 MPa Show Supplier Material materials with Límite elástico of 193 MPa | |
Resistencia a la tracción | 23.0 °C | 469 MPa Show Supplier Material materials with Resistencia a la tracción of 469 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 6 - 8.5 % Show Supplier Material materials with Aluminio of 6 - 8.5 % | ||
Cobre | Balance, including silver | ||
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. | |
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Tube sheets,pickling hooks,impellers,valve seats,chemical plants,pulp mills |