General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 140 [-] Show Supplier Material materials with Dureza Brinell of 140 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 28 % Show Supplier Material materials with Elongación of 28 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 28 % Show Supplier Material materials with Estricción of 28 % | |
Límite elástico | 23.0 °C | 241 MPa Show Supplier Material materials with Límite elástico of 241 MPa | |
Resistencia a la tracción | 23.0 °C | 545 MPa Show Supplier Material materials with Resistencia a la tracción of 545 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 8.5 - 11 % Show Supplier Material materials with Aluminio of 8.5 - 11 % | ||
Cobre | Balance, including silver | ||
Hierro | 0.5 - 1.5 % Show Supplier Material materials with Hierro of 0.5 - 1.5 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Cast iron, Cast iron, Malleable iron, Cast iron to steel, Cast iron to bronze, Steel to bronze, Aluminum bronze, Silicon bronze, Manganese bronze, Cupro-nickel, Copper to steel, Bearings, Bushings, Pump housings, Condenser boxes, Hydraulic pistons, Brake drums, Tractor gear housings, Idler pulleys, Pickling hooks, Paper mill rolls, Motor bases, Tin plate mill rolls, Impellers, Valve seats, Gears, Mixer arms, Press rams, Ship propellers, Lance heads |