General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 185 [-] Show Supplier Material materials with Dureza Brinell of 185 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 27 % Show Supplier Material materials with Elongación of 27 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 38 % Show Supplier Material materials with Estricción of 38 % | |
Límite elástico | 23.0 °C | 386 MPa Show Supplier Material materials with Límite elástico of 386 MPa | |
Resistencia a la tracción | 23.0 °C | 655 MPa Show Supplier Material materials with Resistencia a la tracción of 655 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 7 - 8.5 % Show Supplier Material materials with Aluminio of 7 - 8.5 % | ||
Cobre | Balance, including silver | ||
Hierro | 2 - 4 % Show Supplier Material materials with Hierro of 2 - 4 % | ||
Manganeso | 11 - 14 % Show Supplier Material materials with Manganeso of 11 - 14 % | ||
Níquel | 1.5 - 3 % Show Supplier Material materials with Níquel of 1.5 - 3 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 1.5 % Show Supplier Material materials with Silicona of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Ship propellers, Marine components, Welding cast iron, Joining dissimilar metals |