General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 166 [-] Show Supplier Material materials with Dureza Brinell of 166 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 22 % Show Supplier Material materials with Estricción of 22 % | |
Límite elástico | 23.0 °C | 276 MPa Show Supplier Material materials with Límite elástico of 276 MPa | |
Resistencia a la tracción | 23.0 °C | 621 MPa Show Supplier Material materials with Resistencia a la tracción of 621 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 10 - 11.5 % Show Supplier Material materials with Aluminio of 10 - 11.5 % | ||
Cobre | Balance, including silver | ||
Hierro | 2 - 4.5 % Show Supplier Material materials with Hierro of 2 - 4.5 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Hydraulic pistons, Bearing overlays, Impellers, Turbine runners, Press rams, Cable sheaves, Mill slippers, Valve seats and parts, Breaker blocks, Ceiling machine mandrels, Steel mill rolls, Welding AMPCO® 18 |