General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 160 [-] Show Supplier Material materials with Dureza Brinell of 160 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 17 % Show Supplier Material materials with Estricción of 17 % | |
Límite elástico | 23.0 °C | 324 MPa Show Supplier Material materials with Límite elástico of 324 MPa | |
Resistencia a la tracción | 23.0 °C | 614 MPa Show Supplier Material materials with Resistencia a la tracción of 614 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 9.5 - 11.5 % Show Supplier Material materials with Aluminio of 9.5 - 11.5 % | ||
Cobre | Balance, including silver | ||
Hierro | 2.5 - 5 % Show Supplier Material materials with Hierro of 2.5 - 5 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 1.5 % Show Supplier Material materials with Silicona of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Bronze castings, Strip mill guides, Bearing overlays, Crane contact shoes, Driving sprockets, Drop hammers, Manipulator slides, Gate valves, Sheaves, Pistons, Mill slippers, Turbine runners, Packing glands, Valve seat overlays |